• Scam Alert. Members are reminded to NOT send money to buy anything. Don't buy things remote and have it shipped - go get it yourself, pay in person, and take your equipment with you. Scammers have burned people on this forum. Urgency, secrecy, excuses, selling for friend, newish members, FUD, are RED FLAGS. A video conference call is not adequate assurance. Face to face interactions are required. Please report suspicions to the forum admins. Stay Safe - anyone can get scammed.

TIG rod size

Blue, 2% Lanthinated, a good all around rod without being radioactive ;).

I have both 1/16 and 3/32, currently using 3/32 #6 cup about 13cf argon, usually give myself about 5amps above recommend for headroom, sometime a touch extra heat to start the puddle is great (at least for this beginner), I follow the simple rule 1 amp/0.001" to about 0.140" at which point 150amps seems to work for heavier material. Foot peddle gives me heat control.

I sharpen with my belt grinder and a drill, eyeball point angle.
 
just throwing this out there ,when tig welding you can't use oxyacetylene wire , you'll get porosity ,,, I think its because the wire is not deoxidized
 
I’ve used mig wire before but folded it in half and twisted it with a drill that works good for bodywork.
 
I’ve used tig wire before but folded it in half and twisted it with a drill that works good for bodywork.
TIG wire or MIG wire?
I once tried to twist two 1/32" TIG filler rods to make 1/16" rod and the rods just snapped.
 
...Assuming your talking solid core

MIG/TIG filler, same thing, just different diameters

But oxy filler lacks deoxidizers, and is slightly cheaper as a result (although I would be surprised if anyone carried much for stock these days)....like @hovercraft57 stated is no good for arc welding
 