• Scam Alert. Members are reminded to NOT send money to buy anything. Don't buy things remote and have it shipped - go get it yourself, pay in person, and take your equipment with you. Scammers have burned people on this forum. Urgency, secrecy, excuses, selling for friend, newish members, FUD, are RED FLAGS. A video conference call is not adequate assurance. Face to face interactions are required. Please report suspicions to the forum admins. Stay Safe - anyone can get scammed.

Other Salvaging old iron

Arbutus

Super User
Premium Member
Well I has this offshore angle plate sitting on the shelf taking up room. It has probably been there 10 years or more and the sharpie markings that showed NOT SQUARE! was the reason why it was collecting rust.

It was also an awful machining job, with the slots unevenly spaced and between 11.5 and 13mm wide. One face seemed flat according to the surface plate, but the other face was not square - measuring 89:58" at one end and 89:49 at the other.
Casting inclusion72.jpg
Casting inclusion69.jpeg

But it looked like the casting was sound so I started cleaning it up. The 3/8-16 tapped holes on the ends I added for a clamp system. So far so good, and the tapped holes were nice and smooth, and amazingly there were no hard spots. Seriously I have found pebbles inside cast iron so I didn't have great expectations with this lump. Then I found this...
Casting inclusion67.jpeg
Casting inclusion66.jpeg


The pics show a white plastic inclusion inside the casting which was exposed as I cleaned out the slots. It seems to be about 1/4 dia and less than an inch long. Does anyone have some insight into what that is? It feels chalky, like Bondo. Easily excavated with a screwdriver.

After an hour on the mill and another with the grinder I have a fairly decent angle plate. It will look better after some paint though.

Don
 
Does anyone have some insight into what that is? It feels chalky, like Bondo.

Looks like a gob of silicon adhesive that got into the pour and then got cooked to chalk. Easy to fill the casting void with steel filled epoxy that wouldn't affect its function.
 